OUR TECHNOLOGY


Coating material
Metal, Ceramic
Material feed type
Powder, Wire
Propellant
Compressed air, Fuel
Spray gun temp. (°C)
~3000
Particle velocity (m/s)
~800
Bond strength (Mpa)
~80 (excellent)
Porosity level  (vol%)
~2 (good)
Relative oxidation
Fair

Representative coating materials: WC, Cr3C2, and many more alloy and ceramics